MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam
Categories: Polymer; Adhesive; Thermoplastic; Vinyl (PVC)

Material Notes: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhesive keeps sealant in place during each stage of product assembly. The adhesive is on the non-linear side, making installation easier and quicker.

Features/Benefits:
  • 30% compression provides an excellent seal against light, dust and water in mechanically fastened assemblies
  • Excellent resistance to weather, fungi, and oxidation provides a long sealing life
  • Will not crack in cold temperatures
  • Superb closed cell structure of foam provides a positive seal
  • Low force to compress means faster and easier formation of a positive seal
  • Flexibility facilitates use in radius corners
  • Low density sealant allows easy assembly of large wall systems
Typical Applications: Curtainwall, precast concrete walls, refrigeration, telecommunications, pneumatic system seals, retail weatherstrip, bus and off-road vehicles, air conditioning, environmentally controlled rooms. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/8" to 1/2".)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00350 lb/in³ASTM D1667
Water Absorption 3.0 %% by volume; NTP-35
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 18ASTM D2240
Tensile Strength, Yield 17.0 psiASTM D-412 (Die A)
Elongation at Break 125 %ASTM D-412 (Die A)
Compressive Strength 1.30 psiCompression Deflection, Compressed to 30%.; ASTM D1667
Compressive Modulus 2.00 psiForce to Compress, Value for 30% compression.
Compression Set 8.0 %Constant Deflection, Compressed to 30%.; Norton Test Procedure 37
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.270 BTU-in/hr-ft²-°FASTM-C-518
Maximum Service Temperature, Air 160 °F
Minimum Service Temperature, Air -15.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200)
Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam
Saint-Gobain Norton® V760 High Density Vibration
Saint-Gobain Norton® V740 Multipurpose Pressure Sensitive Adhesive Sealant Foam

PSTGQZ484 / 68998

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.