Treatment required for max strength: Mill Hardened Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98% Stress Relaxation after 1000 hrs @ 200°C: 68% Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 2 Formability Ratio (bad Way): 2 Superficial Hardness: 30N 48-55Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman. Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |