MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 50-3122 One Component Thermally Conductive & Electrically Insulating Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 50-3122 is a one component (no mixing is necessary) epoxy adhesive with a unique combination of physical properties. This adhesive provides both high shear and high peel strengths. It is also able to maintain exceptionally strong bonds over a wide temperature range of -60 to +205°C. 50-3122 is formulated to offer superior resistance to impact, thermal shock, vibration and stress fatigue cracking. This product does not contain solvents and is therefore a 100% solids system. 50-3122 passes NASA’s outgassing requirements per ASTM E595-07. 50-3122 is both a thermally conductive and electrically insulating epoxy adhesive. It is suitable for electronic, electrical, aerospace, appliance, automotive and industrial applications.

Features:

  • High Thermal Conductivity
  • Electrically Insulating
  • Good Chemical Resistance
  • Superior Impact & Thermal Shock Resistance
  • One Component; No Mixing Required

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/cc
Solids Content 100 %
Viscosity 165000 cP
Outgassing - Total Mass Loss 0.020 %CVCM
 0.43 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Tensile Strength 9500 psi
Tensile Modulus 675000 psi
Compressive Strength 16000 psi
Shear Strength 2100 psiLap
Peel Strength 30.0 pliT-Peel, Al to AI
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Dielectric Strength 370 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.44 W/m-K
Maximum Service Temperature, Air 205 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 125 °C
 2.00 hour
@Temperature 100 °C
 5.00 min
@Temperature 175 °C
 10.0 min
@Temperature 160 °C
Shelf Life 6.00 Month
@Temperature 25.0 °C
 12.0 Month
@Temperature 0.000 °C
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX050 / 316727

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.