MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 50-3122 One Component Thermally Conductive & Electrically Insulating Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 50-3122 is a one component (no mixing is necessary) epoxy adhesive with a unique combination of physical properties. This adhesive provides both high shear and high peel strengths. It is also able to maintain exceptionally strong bonds over a wide temperature range of -60 to +205°C. 50-3122 is formulated to offer superior resistance to impact, thermal shock, vibration and stress fatigue cracking. This product does not contain solvents and is therefore a 100% solids system. 50-3122 passes NASA’s outgassing requirements per ASTM E595-07. 50-3122 is both a thermally conductive and electrically insulating epoxy adhesive. It is suitable for electronic, electrical, aerospace, appliance, automotive and industrial applications.

Features:

  • High Thermal Conductivity
  • Electrically Insulating
  • Good Chemical Resistance
  • Superior Impact & Thermal Shock Resistance
  • One Component; No Mixing Required

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/cc
Solids Content 100 %100 %
Viscosity 165000 cP165000 cP
Outgassing - Total Mass Loss 0.020 %0.020 %CVCM
 0.43 %0.43 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Tensile Strength 65.5 MPa9500 psi
Tensile Modulus 4.65 GPa675 ksi
Compressive Strength 110 MPa16000 psi
Shear Strength 14.5 MPa2100 psiLap
Peel Strength 5.26 kN/m30.0 pliT-Peel, Al to AI
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Dielectric Strength 14.6 kV/mm370 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.44 W/m-K9.99 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 205 °C401 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 175 °C
0.0833 hour
@Temperature 347 °F
 10.0 min
@Temperature 160 °C
0.167 hour
@Temperature 320 °F
 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
 120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
Shelf Life  6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
 12.0 Month
@Temperature 0.000 °C
12.0 Month
@Temperature 32.0 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX050 / 316727

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.