MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes: Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/ccASTM D792
Deformation 1.2 %2000 psi 78°F; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2000 psiASTM D1457
Elongation at Break 300 %ASTM D1457
Shear Strength 1500 psi
@Temperature 204 °C
ASTM D732
 1650 psi
@Temperature 149 °C
ASTM D732
 1800 psi
@Temperature 93.3 °C
ASTM D732
 2300 psi
@Temperature 26.7 °C
ASTM D732
Coefficient of Friction, Dynamic 0.1233.3 psi @ 150 fpm
K (wear) Factor 1.00 x 10-10 in³-min/ft-lb-hr
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed Avalon® 89 PTFE
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled
Greene Tweed Avalon® 56 PTFE
Greene Tweed Avalon® 87 PTFE, Glass Filled

PGREEN66 / 42360

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.