MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.27 g/cc2.27 g/ccASTM D792
Deformation 20 %20 %2000 psi 78°F; ASTM D621
 30 %30 %1000 psi 300°F; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 19.48 MPa2825 psiASTM D1457
Elongation at Break 247 %247 %ASTM D1457
Compressive Strength 26.2 MPa3800 psiASTM D695
Shear Strength  14.5 MPa
@Temperature 149 °C
2100 psi
@Temperature 300 °F
ASTM D732
 15.9 MPa
@Temperature 93.3 °C
2300 psi
@Temperature 200 °F
ASTM D732
 17.6 MPa
@Temperature 65.6 °C
2550 psi
@Temperature 150 °F
ASTM D732
 19.3 MPa
@Temperature 37.8 °C
2800 psi
@Temperature 100 °F
ASTM D732
 20.0 MPa
@Temperature 26.7 °C
2900 psi
@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Static 0.100.1033.3 psi
K (wear) Factor 18.1 x 10-8 mm³/N-M9.00 x 10-10 in³-min/ft-lb-hr
 
Descriptive Properties
ColorDark Gray to Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Greene Tweed Avalon® 87 PTFE, Glass Filled
Greene Tweed Avalon® 89 PTFE
Greene Tweed Avalon® 9 PTFE, Graphite Filled

PGREEN62 / 42356

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.