MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici Radilon® NeXTreme RV350HHR 3800 BK Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: High temperature polyamide injection molding grade, 35% glass fiber reinforced. Superior thermal resistance in contact with hot air. Black color.

Suitable for demanding mechanical applications in very severe temperature conditions where the parts must endure long term contact with hot air until 200-230°C. Very good properties retention after aging. Typical applications in automotive are under bonnet components, like turbo air ducts, intercooler end caps. This material can be processed with water conditioned tools.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccDAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 194 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.1 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 12050 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 300 MPa2mm / min. DAM; ISO 178
Flexural Modulus 10000 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 101 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 12.5 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 295 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 252 °CISO 75/2Bf
Flammability, UL94 HB
@Thickness 0.800 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
 
Processing PropertiesOriginal ValueComments
Melt Temperature 305 - 315 °CInjection Molding
Mold Temperature 90.0 - 100 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6933 / 293438

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.