MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici Radilon® NeXTreme RV350HHR 3800 BK Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: High temperature polyamide injection molding grade, 35% glass fiber reinforced. Superior thermal resistance in contact with hot air. Black color.

Suitable for demanding mechanical applications in very severe temperature conditions where the parts must endure long term contact with hot air until 200-230°C. Very good properties retention after aging. Typical applications in automotive are under bonnet components, like turbo air ducts, intercooler end caps. This material can be processed with water conditioned tools.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³DAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.20 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 194 MPa28100 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.1 %3.1 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 12.05 GPa1748 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 300 MPa43500 psi2mm / min. DAM; ISO 178
Flexural Modulus 10.0 GPa1450 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 10.1 J/cm²
@Temperature -30.0 °C
48.1 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.25 J/cm²
@Temperature -30.0 °C
5.95 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 252 °C486 °FISO 75/2Bf
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
 
Processing PropertiesMetricEnglishComments
Melt Temperature 305 - 315 °C581 - 599 °FInjection Molding
Mold Temperature 90.0 - 100 °C194 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6933 / 293438

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.