LNP THERMOCOMP MX06402H compound is based on Polypropylene (PP) resin containing 20% glass fiber. Added features of this grade include: Heat Stabilized, Low Extractables, Healthcare. Features: Low Extractable,Healthcare,High Stiffness,Heat Stabilized,Food Contact Acceptable,Structural Information provided by SABIC |