SABIC® PP grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity.
SABIC® PP PCGR40 is a highly transparent polypropylene random copolymer with good antistatic properties. This grade combines improved aesthetics of the finished articles with low temperature processability and a very good organoleptic performance. Part aesthetics are not affected by the lower temperatures, providing for a broader operating window, enabling short cycle times. SABIC® PP PCGR40 results in excellent demoulding characteristics and has a good stiffness to impact ratio.
Typical applications: SABIC® PP PCGR40 is typically used for injection moulding of housings for empty disposable 3-part syringes. Other applications demanding a high level of transparency and broad processing window are also possible.
Compliance to regulations: SABIC® PP PCGR40 complies with the food contact regulations and the relevant monographs of the US Pharmacopoeia.Information provided by SABIC |