MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PP PCGR40 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity. SABIC® PP PCGR40 is a highly transparent polypropylene random copolymer with good antistatic properties. This grade combines improved aesthetics of the finished articles with low temperature processability and a very good organoleptic performance. Part aesthetics are not affected by the lower temperatures, providing for a broader operating window, enabling short cycle times. SABIC® PP PCGR40 results in excellent demoulding characteristics and has a good stiffness to impact ratio. Typical applications: SABIC® PP PCGR40 is typically used for injection moulding of housings for empty disposable 3-part syringes. Other applications demanding a high level of transparency and broad processing window are also possible. Compliance to regulations: SABIC® PP PCGR40 complies with the food contact regulations and the relevant monographs of the US Pharmacopoeia.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.0 MPa4210 psiISO 527-2 1A
Elongation at Yield 13 %13 %Speed of testing: 50 mm/min; ISO 527-2 1A
Tensile Modulus 1.15 GPa167 ksiSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1A
 2.00 kJ/m²
@Temperature 0.000 °C
0.952 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179/1eA
 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Descriptive Properties
Anti static agentTrue
ClarifiedTrue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11250 / 244717

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.