MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer SLX2071T Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors

Features: Weatherable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 5.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 76.0 MPa50 mm/min; ASTM D638
 76.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 67.0 MPa50 mm/min; ASTM D638
 67.0 MPa50 mm/min; ISO 527
Elongation at Break >= 100 %50 mm/min; ASTM D638
 >= 100 %50 mm/min; ISO 527
Elongation at Yield 6.3 %50 mm/min; ASTM D638
 6.3 %50 mm/min; ISO 527
Tensile Modulus 2340 MPa5 mm/min; ASTM D638
 2340 MPa1 mm/min; ISO 527
Flexural Strength 96.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 96.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2120 MPa1.3 mm/min, 50 mm span; ASTM D790
 2120 MPa2 mm/min; ISO 178
Izod Impact Notched 820 JASTM D256
 140 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 85.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 121 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 134 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 135 °CRate B/50; ASTM D1525
 137 °CRate B/50; ISO 306
 139 °CRate B/120; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 89 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 100 °CCalibrator Temperature
Zone 1 240 - 280 °CProfile Extrusion
Zone 2 240 - 280 °CProfile Extrusion
Zone 3 220 - 240 °CProfile Extrusion
Zone 4 220 - 240 °CProfile Extrusion
Adapter Temperature 220 - 240 °CProfile Extrusion
Die Temperature 245 - 290 °CProfile Extrusion
Melt Temperature 220 - 250 °CProfile Extrusion
Drying Temperature 105 °CProfile Extrusion
Dry Time 2.00 - 3.00 hourProfile Extrusion
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80420 / 288367

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.