MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aclo Accuguard ABS ABS860V0L Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inMD; ASTM D955
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength at Break 27.0 MPa3920 psiASTM D638
Tensile Strength, Yield 41.0 MPa5950 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 1.700 GPa246.5 ksiASTM D638
Flexural Strength 57.0 MPa8270 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 3.58 J/cm6.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C171 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C151 °F
Flammability, UL94 5VA5VA1/10 FSA File #LS66844
 5VA
@Thickness 1.59 mm
5VA
@Thickness 0.0625 in
UL File #E56070, Rating of 5VA with 1/10 FSA File #LS66844

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T65 XF Polycarbonate + ABS
Ecomass® 720ZD91 Tungsten Filled ABS
A. Schulman Diamond DIAMALOY ST4600 TPE/ABS Alloy, Soft Touch Resin
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
PTS Trilac® ABS-HH2350 High Heat ABS

PACLO078 / 22333

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.