MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman Diamond DIAMALOY ST4600 TPE/ABS Alloy, Soft Touch Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Elastomer, TPE

Material Notes: Diamaloy ST4600 material is an alloy of thermoplastics elastomers and ABS, specifically designed to provide a low gloss look and soft touch feel in applications where it is co-extruded or laminated over a ABS (acrylonitrile butadiene styrene) substrate. Diamaloy ST4600 has excellent durability and chemical resistance as well as improved sound dampening when used as a cap over ABS.

Applications: Diamaloy ST4600 alloy resin is recommended for use in interior parts that will have limited exposure to direct UV light such as dashboards, panels and trim. As with any product, use of Diamaloy ST4600 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. The use of Diamaloy ST4600 as the carrier resin for color concentrates is imperative in order to maintain the proper look, feel, and physical performance of the finished product. DIAMOND POLYMERS recommends the Diamaloy ST4600 cap layer should be a minimum of 20 mils in the final part, after thermoforming.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Engineered Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 15 g/10 min
@Load 3.80 kg,
Temperature 230 °C
15 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO-1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ASTM D2240
Instrumented Impact Total Energy 8.00 J5.90 ft-lbASTM D3763
Instrumented Impact Energy at Peak 6.00 J4.43 ft-lbMaximum Energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Flame Spread 42 mm/min1.7 in/minISO 3795
 
Optical PropertiesMetricEnglishComments
Gloss 10 %10 %50 mil Extruded Sheet; 60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accuguard ABS ABS860V0L Flame Retardant
Covestro Bayblend® T65 XF Polycarbonate + ABS
Ecomass® 720ZD91 Tungsten Filled ABS
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
Dow AFFINITY™ KC 8852 Polyolefin Elastomer

PDIAM392 / 126483

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.