MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed Arlon® 1260 Polyketone, Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Arlon® 1260 is a carbon-fiber reinforced version of Arlon 1000 featuring the highest modulus and tensile strength of all the Arlon grades. Designers requiring a low coefficient off thermal expansion often select Arlon 1260.

Arlon 1260 also provides enhanced Tribological properties, reduced friction values and improved wear properties over Arlon 1000. Arlon 1260 is ideal in lubricated bearings and/or moist environments.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9292ASTM D2240
Tensile Strength at Break 230 MPa33400 psiASTM D368
Elongation at Break 1.9 %1.9 %ASTM D638
Tensile Modulus 21.7 GPa3150 ksiASTM D638
Flexural Strength 347 MPa50300 psiASTM D790
Flexural Modulus 19.0 GPa2750 ksiASTM D790
Compressive Strength 262 MPa38000 psiASTM D695
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber
Greene Tweed WR™ FP100 Polyketone, Reinforced
Delrin Delrin® 100 NC010 POM
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber

PGREEN52 / 42346

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.