MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance and lwo extractables similar to PTFE. Providing the lowest temperature sealing properties of any perfluoroelastomer on the market (-22°F, -30°C), Chemraz SD517 is an ideal seal component for sub-ambient mechanical seal applications and is the preferred alternative to encapsulated O-rings. With its white color, Chemraz SD517 meets the needs of applications requiring non-black elastomers.

Chemraz SD517’s many features make it well suited for critical applications and difficult seal replacement locations where maximizing MTBR (mean time between replacement) is paramount.

Chemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes.

This product is FDA and USP Class VI compliant making it an ideal product for electrometric applications requiring regulatory compliance.

Applications:Mechanical seals

  • Valves
  • Pumps
  • Mixers
  • Fermenters
  • Biomedical equipment
  • Couplings

    Information provided by Greene Tweed.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 2.22 g/cc2.22 g/ccASTM D297
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 8080ASTM D2240
    Tensile Strength at Break 11.0 MPa1600 psiASTM D1414
    Tensile Strength, Yield 3.72 MPa540 psi@50% Elongation; ASTM D1414
     7.24 MPa1050 psi@100% Elongation; ASTM D1414
    Compression Set 25 %
    @Temperature 204 °C,
    Time 252000 sec
    25 %
    @Temperature 400 °F,
    Time 70.0 hour
    At 25% deflection; ASTM D395
     
    Thermal PropertiesMetricEnglishComments
    Maximum Service Temperature, Air 220 °C428 °F
    Minimum Service Temperature, Air -30.0 °C-22.0 °F
     
    Compliance PropertiesMetricEnglishComments
    USP Class VI YesYes
     
    Descriptive Properties
    ColorWhite

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
    Greene Tweed CHEMRAZ® 661 Perfluoroelastomer
    Greene Tweed CHEMRAZ® 656 Perfluoroelastomer
    Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
    Greene Tweed CHEMRAZ® 528 Perfluoroelastomer

    PGREEN35 / 42329

    USP Class VI Adhesives
    USP Class VI Approved Adhesives for Medical Device Applications
    Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.