MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed CHEMRAZ® 656 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 656 is a low durometer perfluoroelastomer primarily designed for Bonded Slit Valve gates and special engineered applications such as low sealing forces/tolerance stickups where softer materials aid in the total seal solution. Developed from and advanced polymer utilizing fluoropolymer nano-composite technology particles, Chemraz 656 has very low metallic ion levels and offers resistance to today’s advanced process chemistries. Chemraz 656 is recommended for use in CVD, Etch and diffusion equipment applications.

Applications:

  • Bonded slit valve gates
  • Chamber seals
  • Window seals
  • Gas inlet seals
  • Lid seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.05 g/cc2.05 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 10.37 MPa1504 psiASTM D1414
Tensile Strength, Yield 1.44 MPa209 psi@50% Elongation; ASTM D1414
 2.65 MPa384 psi@100% Elongation; ASTM D1414
Elongation at Break 238 %238 %ASTM D1414
Compression Set 24 %
@Temperature 204 °C,
Time 252000 sec
24 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Greene Tweed CHEMRAZ® SD585 Perfluoroelastomer
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer

PGREEN32 / 42326

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.