MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed CHEMRAZ® E38 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excellent chemical compatibility and withstands a variety of aggressive chemicals. Available in an infinite range of geometries and cross sections, this material offers the diversity required for a variety of dynamic or static dry processing applications. Recommended for slit valves, Chemraz E38 remains stable at service temperatures as high as 260°C (500°F) where high sealing loads are not used.

Applications:

  • Bonded gate seals
  • Chamber seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.99 g/cc1.99 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 15.2 MPa2200 psiASTM D1414
Tensile Strength, Yield 2.83 MPa410 psi@50% Elongation; ASTM D1414
 7.58 MPa1100 psi@100% Elongation; ASTM D1414
Elongation at Break 150 %150 %ASTM D1414
Compression Set 21 %
@Temperature 204 °C,
Time 252000 sec
21 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Greene Tweed CHEMRAZ® SD585 Perfluoroelastomer
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer
Greene Tweed CHEMRAZ® 656 Perfluoroelastomer

PGREEN34 / 42328

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.