MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Duratherm HTO Heat Transfer Fluid
Categories: Fluid

Material Notes: Duratherm HTO is engineered for many years of service and it’s ideal for a wide range of closed to atmosphere (inertly sealed) applications including paint, rubber, paper mill calendars, board plants, roofing, textiles, laundry, refineries and asphalt production. Duratherm HTO’s uses highly refined base stocks that ensures excellent thermal stability. Its low volatility minimizes vapor pressure at elevated temperatures. Duratherm HTO contains antioxidants, metal deactivators and corrosion inhibitors to enhance the fluid’s longevity. Duratherm HTO is environmentally friendly, non-toxic, non-hazardous and non-reportable. Duratherm HTO poses no ill effect to worker safety. Duratherm HTO can easily be disposed of with other waste oils.

Information provided by Duratherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 39.4 lb/ft³
@Temperature 315 °C
 39.4 lb/ft³
@Temperature 316 °C
ASTM D1298
 41.7 lb/ft³
@Temperature 260 °C
ASTM D1298
 43.1 lb/ft³
@Temperature 225 °C
 50.6 lb/ft³
@Temperature 38.0 °C
ASTM D1298
 51.9 lb/ft³
@Temperature 5.00 °C
Viscosity 0.49 cP
@Temperature 315 °C
Dynamic
 0.92 cP
@Temperature 225 °C
Dynamic
 250.63 cP
@Temperature 5.00 °C
Dynamic
Kinematic Viscosity 0.74 cSt
@Temperature 315 °C
 1.26 cSt
@Temperature 225 °C
 6.34 cSt
@Temperature 100 °C
ASTM D445
 39.35 cSt
@Temperature 40.0 °C
ASTM D445
 286.16 cSt
@Temperature 5.00 °C
Molecular Weight 371 g/molAverage
Vapor Pressure 0.000 atm
@Temperature 38.0 °C
ASTM D2879
 0.000 atm
@Temperature 5.00 °C
 0.00800 atm
@Temperature 225 °C
 0.0230 atm
@Temperature 260 °C
ASTM D2879
 0.0990 atm
@Temperature 316 °C
ASTM D2879
 0.100 atm
@Temperature 315 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1011 µm/m-°C
Specific Heat Capacity 0.00180 J/g-°C
@Temperature 5.00 °C
 0.00250 J/g-°C
@Temperature 225 °C
 0.00280 J/g-°C
@Temperature 315 °C
 1.892 J/g-°C
@Temperature 38.0 °C
 2.587 J/g-°C
@Temperature 260 °C
 2.763 J/g-°C
@Temperature 316 °C
Thermal Conductivity 0.121 W/m-K
@Temperature 316 °C
 0.121 W/m-K
@Temperature 315 °C
 0.124 W/m-K
@Temperature 260 °C
 0.126 W/m-K
@Temperature 225 °C
 0.136 W/m-K
@Temperature 38.0 °C
 0.138 W/m-K
@Temperature 0.000 °C
Distillation Temperature 372 - 455 °C10% to 90% range; ASTM D2887
Maximum Service Temperature, Air 315 °CBulk/Use Temp.
 332 °CFilm Temp.
Pour Point -15.0 °CASTM D97
Flash Point 218 °CASTM D92
Ignition Temperature 360 °CASTM E-659-78
 
Descriptive Properties
AppearanceClear and bright liquid
Fire Point (°C)231ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDURA675 / 287873

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.