Physical Properties | Metric | English | Comments |
---|
Density | 0.631 g/cc @Temperature 315 °C | 0.0228 lb/in³ @Temperature 599 °F |
| 0.631 g/cc @Temperature 316 °C | 0.0228 lb/in³ @Temperature 601 °F |
| 0.668 g/cc @Temperature 260 °C | 0.0241 lb/in³ @Temperature 500 °F |
| 0.690 g/cc @Temperature 225 °C | 0.0249 lb/in³ @Temperature 437 °F |
| 0.811 g/cc @Temperature 38.0 °C | 0.0293 lb/in³ @Temperature 100 °F |
| 0.831 g/cc @Temperature 5.00 °C | 0.0300 lb/in³ @Temperature 41.0 °F |
Viscosity | 0.49 cP @Temperature 315 °C | 0.49 cP @Temperature 599 °F |
| 0.92 cP @Temperature 225 °C | 0.92 cP @Temperature 437 °F |
| 250.63 cP @Temperature 5.00 °C | 250.63 cP @Temperature 41.0 °F |
Kinematic Viscosity | 0.74 cSt @Temperature 315 °C | 0.74 cSt @Temperature 599 °F |
| 1.26 cSt @Temperature 225 °C | 1.26 cSt @Temperature 437 °F |
| 6.34 cSt @Temperature 100 °C | 6.34 cSt @Temperature 212 °F |
| 39.35 cSt @Temperature 40.0 °C | 39.35 cSt @Temperature 104 °F |
| 286.16 cSt @Temperature 5.00 °C | 286.16 cSt @Temperature 41.0 °F |
Molecular Weight | 371 g/mol | 371 g/mol |
Vapor Pressure | 0.000 bar @Temperature 38.0 °C | 0.000 torr @Temperature 100 °F |
| 0.000 bar @Temperature 5.00 °C | 0.000 torr @Temperature 41.0 °F |
| 0.00811 bar @Temperature 225 °C | 6.08 torr @Temperature 437 °F |
| 0.0233 bar @Temperature 260 °C | 17.5 torr @Temperature 500 °F |
| 0.100 bar @Temperature 316 °C | 75.2 torr @Temperature 601 °F |
| 0.101 bar @Temperature 315 °C | 76.0 torr @Temperature 599 °F |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 1011 µm/m-°C | 561.7 µin/in-°F |
Specific Heat Capacity | 0.00180 J/g-°C @Temperature 5.00 °C | 0.000430 BTU/lb-°F @Temperature 41.0 °F |
| 0.00250 J/g-°C @Temperature 225 °C | 0.000598 BTU/lb-°F @Temperature 437 °F |
| 0.00280 J/g-°C @Temperature 315 °C | 0.000669 BTU/lb-°F @Temperature 599 °F |
| 1.892 J/g-°C @Temperature 38.0 °C | 0.4522 BTU/lb-°F @Temperature 100 °F |
| 2.587 J/g-°C @Temperature 260 °C | 0.6183 BTU/lb-°F @Temperature 500 °F |
| 2.763 J/g-°C @Temperature 316 °C | 0.6604 BTU/lb-°F @Temperature 601 °F |
Thermal Conductivity | 0.121 W/m-K @Temperature 316 °C | 0.840 BTU-in/hr-ft²-°F @Temperature 601 °F |
| 0.121 W/m-K @Temperature 315 °C | 0.840 BTU-in/hr-ft²-°F @Temperature 599 °F |
| 0.124 W/m-K @Temperature 260 °C | 0.861 BTU-in/hr-ft²-°F @Temperature 500 °F |
| 0.126 W/m-K @Temperature 225 °C | 0.874 BTU-in/hr-ft²-°F @Temperature 437 °F |
| 0.136 W/m-K @Temperature 38.0 °C | 0.944 BTU-in/hr-ft²-°F @Temperature 100 °F |
| 0.138 W/m-K @Temperature 0.000 °C | 0.958 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
Distillation Temperature | 372 - 455 °C | 702 - 851 °F |
Maximum Service Temperature, Air | 315 °C | 599 °F |
| 332 °C | 630 °F |
Pour Point | -15.0 °C | 5.00 °F |
Flash Point | 218 °C | 424 °F |
Ignition Temperature | 360 °C | 680 °F |
|
Descriptive Properties |
---|
Appearance | Clear and bright liquid |
Fire Point (°C) | 231 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.