MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Malleable iron casting, Class 90001
Categories: Metal; Ferrous Metal; Cast Iron; Malleable Iron

Material Notes: Pearlitic and Martensitic. Temper carbon in necessary matrix without primary cementite or graphite. Applications include general engineering service at normal and elevated temperatures. Dimensional tolerance range for castings is stipulated.

Key Words: ASTM A220, ANSI G48.2, MIL-I-1444B, Malleable iron casting grade 90001, pearlitic, martensitic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 269 - 321269 - 321
Hardness, Knoop 329329Estimated from Brinell
Hardness, Rockwell C 27.927.9Estimated from Brinell
Hardness, Vickers 313313Estimated from Brinell
Tensile Strength, Ultimate 724 MPa105000 psi
Tensile Strength, Yield 621 MPa90100 psi
Elongation at Break 1.0 %1.0 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.0 - 2.7 %2.0 - 2.7 %
Iron, Fe 95 %95 %
Manganese, Mn 0.25 - 1.25 %0.25 - 1.25 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 1.0 - 1.75 %1.0 - 1.75 %
Sulfur, S 0.030 - 0.18 %0.030 - 0.18 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Malleable iron casting, Class 32510
Malleable iron casting, Class M5503 liquid quenched and tempered
Overview of materials for Malleable Iron
ASTM A197 malleable iron casting
Malleable iron casting, Class 35018

MMFE11 / 12433

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.