MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Malleable iron casting, Class 32510
Categories: Metal; Ferrous Metal; Cast Iron; Malleable Iron

Material Notes: Temper carbon and ferrite microstructure. Applications include general engineering service at normal and elevated temperatures for good machinability and excellent shock resistance.

Key Words: ASTM A47, ASTM A338, ANSI G48.1, FED QQ-I-666c, Malleable iron casting grade 32510, ferritic, good machinability, shock resistant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 156<= 156
Hardness, Knoop 173173Estimated from Brinell
Hardness, Vickers 161161Estimated from Brinell
Tensile Strength, Ultimate 345 MPa50000 psi
Tensile Strength, Yield 224 MPa32500 psi
Elongation at Break 10 %10 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.3 - 2.7 %2.3 - 2.7 %
Iron, Fe 96 %96 %
Manganese, Mn 0.25 - 0.55 %0.25 - 0.55 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 1.0 - 1.75 %1.0 - 1.75 %
Sulfur, S 0.030 - 0.18 %0.030 - 0.18 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Malleable iron casting, Class 35018
Ductile Iron grade 65-45-12
ASTM A197 malleable iron casting
Overview of materials for Malleable Iron
Malleable iron casting, Class 40010

MMFE01 / 12423

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.