MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sandvik 19.LNbTi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.LNbTi welding wire has excellent resistance to oxidation in air and in Sulphur containing combustion gases. Its strength at high temperatures is enhanced by the addition of Ti and Nb. It is suitable for joining similar parent metals in, for example the high temperature part of exhaust systems for the automotive industry. It is also suitable for overlay welding, where oxidation resistance is required.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.025 %<= 0.025 %
Chromium, Cr 19 %19 %
Manganese, Mn 0.50 %0.50 %
Niobium, Nb (Columbium, Cb) 0.40 %0.40 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.80 %0.80 %
Sulfur, S <= 0.015 %<= 0.015 %
Titanium, Ti <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMSX-2 Nickel Alloy Composition Spec
Sandvik Sanicro 68HP Welding Wire
Sandvik 19.9 Welding Wire
PWA 1480 Nickel Alloy Composition Spec
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced

NSANDV5100 / 199664

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.