Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
2779
materials in the category
Alloy Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
2779
Results
-- Page
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
of
56
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for AISI 4000 Series Steel
2
Overview of materials for AISI 5000 Series Steel
3
Overview of materials for AISI 6000 Series Steel
4
Overview of materials for AISI 8000 Series Steel
5
Overview of materials for AISI 9000 Series Steel
6
Overview of materials for Low Alloy Steel
7
Overview of materials for Medium Alloy Steel
8
AISI 1330 Steel
9
AISI 1330H Steel
10
AISI 1335 Steel
11
AISI 1335H Steel
12
AISI 1345 Steel
13
AISI 1345H Steel
14
AISI 1340 Steel, annealed at 800°C, furnace cooled 11°C/hour to 600°C, air cooled, 25 mm (1 in.) round
15
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
16
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round
17
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 50 mm (2 in.) round
18
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 100 mm (4 in.) round
19
AISI 1340 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
20
AISI 1340 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
21
AISI 1340 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
22
AISI 1340 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
23
AISI 1340 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
24
AISI 1340 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
25
AISI 1340 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
26
AISI 1340 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
27
AISI 1340 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
28
AISI 1340 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
29
AISI 1340 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 50 mm (2 in.) round
30
AISI 1340 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 100 mm (4 in.) round
31
AISI 1340H Steel, annealed at 800°C, furnace cooled 11°C/hour to 600°C, air cooled, 25 mm (1 in.) round
32
AISI 1340H Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
33
AISI 1340H Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round
34
AISI 1340H Steel, normalized at 870°C (1600°F), air cooled, 50 mm (2 in.) round
35
AISI 1340H Steel, normalized at 870°C (1600°F), air cooled, 100 mm (4 in.) round
36
AISI 1340H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
37
AISI 1340H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
38
AISI 1340H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
39
AISI 1340H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
40
AISI 1340H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
41
AISI 1340H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
42
AISI 1340H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
43
AISI 1340H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
44
AISI 1340H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
45
AISI 1340H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
46
AISI 1340H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 50 mm (2 in.) round
47
AISI 1340H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 100 mm (4 in.) round
48
AISI Grade 18Ni (350) Maraging Steel solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 6 hours
49
AISI 2330 Steel (UNS G23300)
50
AISI 2515 Steel (UNS G25150)
Found
2779
Results
-- Page
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
of
56
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.