MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for injection moulding. The products made out of PRE-ELEC® ESD 7140 are washable, reusable and recyclable. Surface resistance values of 108 ohms (IEC 61340-5-1, EOS/ESD S11.11-1993) can be achieved with optimum processing parameters.

Applications: Trays, tote bins, crates and technical parts which give permanent ESD protection for the electronics, medical, pharmaceutical and paper handling industries. PRE-ELEC® ESD 7140 can be coloured into various bright colours.
Test Specimen: 10[mm] wide moulded rod

Information from Premix OY

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Thickness 102 microns4.00 mil
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4
Melt Flow 32 g/10 min
@Load 5.00 kg,
Temperature 200 °C
32 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 26.0 MPa3770 psiISO 527
Tensile Strength, Yield 33.0 MPa4790 psiISO 527
Elongation at Break 38 %38 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Modulus of Elasticity 1.70 GPa247 ksiISO 178
Izod Impact, Notched (ISO)  9.00 kJ/m²
@Thickness 4.00 mm,
Temperature -20.0 °C
4.28 ft-lb/in²
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
 24.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
11.4 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO)  NB
@Thickness 4.00 mm,
Temperature 23.0 °C
NB
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
 NB
@Thickness 4.00 mm,
Temperature -20.0 °C
NB
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+9 ohm<= 1.00e+9 ohmTest specimen: 100mm x 100mm x 3mm molded plaque; ISO IEC 61340-5-1
Static Decay <= 2.0 sec<= 2.0 secFrom 1000 V down to 100 V, Test specimen: 100mm x 100mm x 3mm molded plaque; ISO IEC 61340-5-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °F75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °F75/Method Af
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 220 °C<= 428 °F
Melt Temperature 190 - 210 °C374 - 410 °F
Mold Temperature 30.0 - 70.0 °C86.0 - 158 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °FPre-drying in a dehumidifier
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.15 %<= 0.15 %when produced
Injection Pressure 75.2 - 120 MPa10900 - 17400 psi
Hold Pressure 40.0 - 60.0 MPa5800 - 8700 psiPost Pressure
Shelf Life 12.0 Month12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
ColorWhitish
Injection SpeedModerate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound

PPRELZ014 / 122149

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.