MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance between 104-107 ohms PRE-ELEC® PP 1399 has an excellent balance of mechanical properties and is easy to injection mould.

Applications: Injection moulded crates, boxes, pallets and tote bins for electronic, automotive and chemical industry to prevent static charges.

Processing: PRE-ELEC® PP 1399 compound can be processed in the injection moulding machines using normal processing conditions as with polypropylene.
Test Specimen: 10[mm] wide moulded rod

Information from Premix OY

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
Thickness 102 microns4.00 mil
Linear Mold Shrinkage 0.012 - 0.018 cm/cm0.012 - 0.018 in/inISO 294-4
Melt Flow  4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 20 g/10 min
@Load 5.00 kg,
Temperature 230 °C
20 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9696ISO 868
Hardness, Shore D 7171ISO 868
Tensile Strength 18.0 MPa2610 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break 30 %30 %ISO 527
Elongation at Yield 10 %10 %ISO 527
Flexural Modulus 1.40 GPa203 ksiISO 178
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Thickness 4.00 mm,
Temperature -20.0 °C
1.43 ft-lb/in²
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
 NB
@Thickness 4.00 mm,
Temperature 23.0 °C
NB
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO)  NB
@Thickness 4.00 mm,
Temperature 23.0 °C
NB
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
 NB
@Thickness 4.00 mm,
Temperature -20.0 °C
NB
@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Charpy Impact Unnotched  NB
@Thickness 102 mm,
Temperature 23.0 °C
NB
@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
 NB
@Thickness 102 mm,
Temperature -20.0 °C
NB
@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
Charpy Impact, Notched  0.600 J/cm²
@Thickness 102 mm,
Temperature -20.0 °C
2.86 ft-lb/in²
@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
 4.00 J/cm²
@Thickness 102 mm,
Temperature 23.0 °C
19.0 ft-lb/in²
@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 1.00e+7 ohm-cm1000 - 1.00e+7 ohm-cmISO D-257
Surface Resistance 10000 - 1.00e+7 ohm10000 - 1.00e+7 ohmISO IEC 61340-5-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °F75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °F75/Method Af
Vicat Softening Point 150 °C302 °FISO 306/A50
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 260 °C392 - 500 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 60.0 - 80.0 °C140 - 176 °FPre-drying
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 60.0 - 80.0 MPa8700 - 11600 psi
Shelf Life 12.0 Month12.0 MonthNormal Storing Conditions
 
Descriptive Properties
Injection SpeedModerate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound
Covestro Makrolon® LED2245 Polycarbonate
Covestro Makrolon® GF8002 Polycarbonate, 15% Glass Filled

PPRELZ031 / 122166

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.