Physical Properties | Metric | English | Comments |
---|
Density | 0.0520 g/cc | 0.00188 lb/in³ |
Moisture Absorption at Equilibrium | 2.4 % | 2.4 % |
Cell Length | 0.250 mm | 0.00984 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore OO | 79 | 79 |
Tensile Strength | 1.30 MPa | 189 psi |
Elongation at Break | 70 % | 70 % |
Flexural Modulus | 0.000200 GPa @Temperature 200 °C | 0.0290 ksi @Temperature 392 °F |
| 0.000200 GPa @Temperature 200 °C | 0.0290 ksi @Temperature 392 °F |
| 0.00100 GPa @Temperature 150 °C | 0.145 ksi @Temperature 302 °F |
| 0.00100 GPa @Temperature 150 °C | 0.145 ksi @Temperature 302 °F |
| 0.00150 GPa @Temperature 100 °C | 0.218 ksi @Temperature 212 °F |
| 0.00200 GPa @Temperature 100 °C | 0.290 ksi @Temperature 212 °F |
| 0.00200 GPa @Temperature 0.000 °C | 0.290 ksi @Temperature 32.0 °F |
| 0.00200 GPa @Temperature 50.0 °C | 0.290 ksi @Temperature 122 °F |
| 0.00700 GPa @Temperature 50.0 °C | 1.02 ksi @Temperature 122 °F |
| 0.0100 GPa @Temperature 0.000 °C | 1.45 ksi @Temperature 32.0 °F |
| 0.0110 GPa @Temperature -40.0 °C | 1.60 ksi @Temperature -40.0 °F |
| 0.0120 GPa @Temperature -40.0 °C | 1.74 ksi @Temperature -40.0 °F |
Compressive Yield Strength | 0.170 MPa @Strain 10 % | 24.7 psi @Strain 10 % |
| 0.190 MPa @Strain 25 % | 27.6 psi @Strain 25 % |
| 0.225 MPa @Strain 40 % | 32.6 psi @Strain 40 % |
| 0.280 MPa @Strain 50 % | 40.6 psi @Strain 50 % |
Tear Strength | 3.00 kN/m | 17.1 pli |
Compression Set | 12 % @Time 79200 sec, Strain 25 % | 12 % @Time 22.0 hour, Strain 25 % |
| 14 % @Time 79200 sec, Strain 25 % | 14 % @Time 22.0 hour, Strain 25 % |
| 24 % @Time 79200 sec, Strain 50 % | 24 % @Time 22.0 hour, Strain 50 % |
| 29 % @Time 79200 sec, Strain 50 % | 29 % @Time 22.0 hour, Strain 50 % |
|
Thermal Properties | Metric | English | Comments |
---|
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F |
| 0.0381 W/m-K | 0.264 BTU-in/hr-ft²-°F |
| 0.0405 W/m-K | 0.281 BTU-in/hr-ft²-°F |
| 0.0420 W/m-K | 0.291 BTU-in/hr-ft²-°F |
| 0.0463 W/m-K | 0.321 BTU-in/hr-ft²-°F |
| 0.0512 W/m-K | 0.355 BTU-in/hr-ft²-°F |
Maximum Service Temperature, Air | 205 °C | 401 °F |
Shrinkage | <= 2.0 % @Temperature 130 °C, Time 3.60e+6 sec | <= 2.0 % @Temperature 266 °F, Time 1000 hour |
| <= 2.0 % @Temperature 160 °C, Time 36000 sec | <= 2.0 % @Temperature 320 °F, Time 10.0 hour |
| <= 2.0 % @Temperature 190 °C, Time 36000 sec | <= 2.0 % @Temperature 374 °F, Time 10.0 hour |
| <= 3.0 % @Temperature 160 °C, Time 360000 sec | <= 3.0 % @Temperature 320 °F, Time 100 hour |
| <= 4.0 % @Temperature 160 °C, Time 3.60e+6 sec | <= 4.0 % @Temperature 320 °F, Time 1000 hour |
| <= 5.0 % @Temperature 190 °C, Time 360000 sec | <= 5.0 % @Temperature 374 °F, Time 100 hour |
|
Descriptive Properties |
---|
Flammability | Automotive: FMVSS.302 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.