MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermal Ceramics Min-K Mid Range Insulating Tape
Categories: Ceramic

Material Notes: Flexible Min-K insulating tape is constructed of Min-K core material enclosed with heat-resistant fabrics stitched in parallel pattern. Available in a range of widths and thicknesses, the tape provides the many advantages of flexible Min-K blankets, enabling it to achieve maximum insulating effect in minimum space.

Min-K tape has a lower thermal conductivity than the molecular conductivity of still air, as well as significantly reduced conductivity at high attitudes. It is particularly effective in controlling thermal transients and provides high resistance to potential damage from compression and vibration.

Features:

  • Easy to use
  • Flexible
  • Variety of thicknesses and sizes
  • Applications

  • Fuel, oil and hydraulic lines
  • Ducts
  • Compressors and de-icing equipment
  • High temperature tubing and piping systems
  • A variety of hard-to-insulate areas where weight is critical and working space is minimal
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.256 g/cc0.00925 lb/in³
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0331 W/m-K
    @Temperature 204 °C
    0.230 BTU-in/hr-ft²-°F
    @Temperature 400 °F
     0.0403 W/m-K
    @Temperature 316 °C
    0.280 BTU-in/hr-ft²-°F
    @Temperature 600 °F
     0.0490 W/m-K
    @Temperature 427 °C
    0.340 BTU-in/hr-ft²-°F
    @Temperature 800 °F
     0.0576 W/m-K
    @Temperature 538 °C
    0.400 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    Maximum Service Temperature, Air 982 °C1800 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Thermal Ceramics Min-K 2000 Data Recorder Molded Min-K Insulation
    3M Nextel™ 610 Composite Ceramic Fiber
    Thermal Ceramics Min-K Type HT Insulating Tape
    Thermal Ceramics Min-K 1303 Data Recorder Molded Min-K Insulation
    Thermal Ceramics Min-K Standard Insulating Tape

    CTHERM219 / 2539

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.