Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Cast Film
- Co-Extrusion Films
- Foams
- High Clarity Film
- Lamination Film
Information provided by ExxonMobil |