MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Categories: Polymer; Thermoplastic; EMAAA Terpolymer

Material Notes: LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.

Main applications

LOTADER 3210 is a versatile adhesive for extrusion coating or lamination, designed as:

  • Concentrate to be used in dry blend with LDPE. LOTADER 3210 improves adhesion of LDPE on alu foils, metallized or primerized films.
  • Ready for use resin to be used pure. LOTADER 3210 gives excellent adhesion on substrates like alu foil, metallized plastics, paper, board, PE and some plastic films like BOPP.
  • Coextrusion tie layer for PE/PA in extrusion coating process.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc
@Temperature 23.0 °C
0.0340 lb/in³
@Temperature 73.4 °F
ISO 1183
Butyl Acrylate Content 6.0 %6.0 %IRTF (internal)
Melt Index of Compound 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ASTM D2240
Tensile Strength at Break 12.0 MPa1740 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
Flexural Modulus 0.120 GPa17.4 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 107 °C225 °FDSC
Vicat Softening Point 76.0 °C
@Load 0.999 kg
169 °F
@Load 2.20 lb
ASTM D1525
Brittleness Temperature <= -50.0 °C<= -58.0 °FASTM D726
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 330 °C518 - 626 °F
 
Descriptive Properties
Maleic Anhydride Content (%)3.1IRTF (internal)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PARKG180 / 80076

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.