MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Fiber Filled

Material Notes: Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.

Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compounds. It has superior surface finish, comparable with General Purpose phenolics. Because of the nature of the fiber used, this compound has very good latitude in injection molding situations.

Data provided by Plaslok Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Apparent Bulk Density 0.500 g/cc0.0181 lb/in³ASTM D1895
Water Absorption 0.40 %0.40 %ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inInjection; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 56.0 MPa8120 psiASTM D638
Flexural Yield Strength 86.0 MPa12500 psiASTM D790
Flexural Modulus 6.90 GPa1000 ksiASTM D790
Compressive Yield Strength 235 MPa34100 psiASTM D695
Izod Impact, Notched 0.210 J/cm0.393 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 12.2 kV/mm310 kV/inASTM D149
Comparative Tracking Index 180 V180 VUL 746
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 150 °C
@Thickness 1.60 mm
302 °F
@Thickness 0.0630 in
UL RTI, Mechanical with Impact 150 °C
@Thickness 1.60 mm
302 °F
@Thickness 0.0630 in
UL RTI, Mechanical without Impact 150 °C
@Thickness 1.60 mm
302 °F
@Thickness 0.0630 in
Flammability, UL94  V-0
@Thickness 6.10 mm
V-0
@Thickness 0.240 in
 V-0
@Thickness 6.10 mm
V-0
@Thickness 0.240 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman Premi-Glas® 2100-22CRSX Polyester BMC
A. Schulman Premi-Glas® 2100-20CRSX Polyester BMC

PZ90P22 / 21107

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.