MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Thermoset Polyester Glass Filled BMC
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyester Glass Filled BMC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 - 2.20 g/cc0.0506 - 0.0795 lb/in³Average value: 1.85 g/cc Grade Count:260
Filler Content 5.00 - 35.0 %5.00 - 35.0 %Average value: 19.1 % Grade Count:57
Water Absorption 0.000 - 0.600 %0.000 - 0.600 %Average value: 0.204 % Grade Count:221
Moisture Absorption at Equilibrium 0.100 - 0.300 %0.100 - 0.300 %Average value: 0.213 % Grade Count:4
Linear Mold Shrinkage -0.000500 - 0.0600 cm/cm-0.000500 - 0.0600 in/inAverage value: 0.00271 cm/cm Grade Count:226
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 10.0 - 80.010.0 - 80.0Average value: 44.5 Grade Count:89
Hardness, Rockwell E 40.0 - 52.040.0 - 52.0Average value: 47.4 Grade Count:7
Hardness, Rockwell M 80.080.0Average value: 80.0 Grade Count:23
Ball Indentation Hardness 250 - 425 MPa36300 - 61600 psiAverage value: 318 MPa Grade Count:6
Tensile Strength, Ultimate 20.0 - 621 MPa2900 - 90100 psiAverage value: 65.9 MPa Grade Count:206
Tensile Strength, Yield 20.0 - 415 MPa2900 - 60200 psiAverage value: 57.8 MPa Grade Count:26
Elongation at Break 0.000 - 1.60 %0.000 - 1.60 %Average value: 0.267 % Grade Count:40
Modulus of Elasticity 6.00 - 25.0 GPa870 - 3630 ksiAverage value: 13.6 GPa Grade Count:94
Flexural Yield Strength 38.0 - 793 MPa5510 - 115000 psiAverage value: 132 MPa Grade Count:266
Flexural Modulus 4.00 - 33.8 GPa580 - 4900 ksiAverage value: 12.0 GPa Grade Count:229
 5.00 - 5.00 GPa
@Temperature 150 - 150 °C
725 - 725 ksi
@Temperature 302 - 302 °F
Average value: 7.64 GPa Grade Count:1
 8.96318 - 8.96318 GPa
@Temperature 150 - 150 °C
1300.02 - 1300.02 ksi
@Temperature 302 - 302 °F
Average value: 7.64 GPa Grade Count:1
 8.96318 - 8.96318 GPa
@Thickness 0.500 - 0.500 mm
1300.02 - 1300.02 ksi
@Thickness 0.0197 - 0.0197 in
Average value: 7.64 GPa Grade Count:1
Compressive Yield Strength 55.0 - 552 MPa7980 - 80000 psiAverage value: 162 MPa Grade Count:155
 124.106 - 137.895 MPa
@Temperature 149 - 260 °C
18000.0 - 20000.0 psi
@Temperature 300 - 500 °F
Average value: 132 MPa Grade Count:2
Compressive Modulus 21.4 - 24.1 GPa3100 - 3500 ksiAverage value: 23.0 GPa Grade Count:3
Poissons Ratio 0.270 - 0.3000.270 - 0.300Average value: 0.298 Grade Count:43
Shear Modulus 3.50 - 9.62 GPa508 - 1400 ksiAverage value: 5.20 GPa Grade Count:39
Shear Strength 14.0 - 100 MPa2030 - 14500 psiAverage value: 47.6 MPa Grade Count:46
Izod Impact, Notched 0.427 - 21.4 J/cm0.800 - 40.1 ft-lb/inAverage value: 3.73 J/cm Grade Count:162
Izod Impact, Unnotched 0.850 - 26.7 J/cm1.59 - 50.0 ft-lb/inAverage value: 5.23 J/cm Grade Count:39
Izod Impact, Unnotched (ISO) 10.0 - 44.0 kJ/m²4.76 - 20.9 ft-lb/in²Average value: 33.8 kJ/m² Grade Count:6
Charpy Impact Unnotched 0.300 - 5.00 J/cm²1.43 - 23.8 ft-lb/in²Average value: 2.19 J/cm² Grade Count:50
Charpy Impact, Notched 0.160 - 37.2 J/cm²0.761 - 177 ft-lb/in²Average value: 2.98 J/cm² Grade Count:65
Crush Resistance 3630 - 27200 kg8000 - 60000 lb (mass)Average value: 11500 kg Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 - 2.20e+16 ohm-cm1.00e+6 - 2.20e+16 ohm-cmAverage value: 1.12e+15 ohm-cm Grade Count:80
Surface Resistance 1.00e+8 - 1.79e+15 ohm1.00e+8 - 1.79e+15 ohmAverage value: 1.74e+14 ohm Grade Count:81
Insulation Resistance 5.00e+8 ohm5.00e+8 ohmAverage value: 5.00e+8 ohm Grade Count:5
Dielectric Constant 4.00 - 19.14.00 - 19.1Average value: 4.97 Grade Count:84
Dielectric Strength 2.61 - 40.0 kV/mm66.3 - 1020 kV/inAverage value: 16.8 kV/mm Grade Count:176
Dielectric Breakdown 21800 - 23000 V21800 - 23000 VAverage value: 22600 V Grade Count:5
 >= 35000 V
@Temperature 90.0 - 90.0 °C
>= 35000 V
@Temperature 194 - 194 °F
Average value: 35000 V Grade Count:5
Dissipation Factor 0.00500 - 0.4000.00500 - 0.400Average value: 0.0308 Grade Count:79
Dielectric Loss Index 0.0110 - 0.01500.0110 - 0.0150Average value: 0.0130 Grade Count:4
Arc Resistance 104 - 285 sec104 - 285 secAverage value: 184 sec Grade Count:173
High Voltage Arc Resistance to Ignition (HVAR) 300 sec300 secAverage value: 300 sec Grade Count:6
Track Resistance 16.7 - 90000 sec16.7 - 90000 secAverage value: 19000 sec Grade Count:41
Comparative Tracking Index 300 - 601 V300 - 601 VAverage value: 586 V Grade Count:93
Hot Wire Ignition, HWI 15.0 - 120 sec15.0 - 120 secAverage value: 101 sec Grade Count:6
High Amp Arc Ignition, HAI 30.0 - 120 arcs30.0 - 120 arcsAverage value: 99.4 arcs Grade Count:6
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minAverage value: 5.00 mm/min Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 - 40.0 µm/m-°C3.33 - 22.2 µin/in-°FAverage value: 18.0 µm/m-°C Grade Count:47
 10.0 - 20.0 µm/m-°C
@Temperature 50.0 - 100 °C
5.56 - 11.1 µin/in-°F
@Temperature 122 - 212 °F
Average value: 15.0 µm/m-°C Grade Count:8
CTE, linear, Transverse to Flow 25.0 - 27.0 µm/m-°C13.9 - 15.0 µin/in-°FAverage value: 25.7 µm/m-°C Grade Count:14
Specific Heat Capacity 1.10 - 1.51 J/g-°C0.263 - 0.360 BTU/lb-°FAverage value: 1.16 J/g-°C Grade Count:32
Thermal Conductivity 0.173 - 1.20 W/m-K1.20 - 8.33 BTU-in/hr-ft²-°FAverage value: 0.609 W/m-K Grade Count:55
Maximum Service Temperature, Air 130 - 288 °C266 - 550 °FAverage value: 179 °C Grade Count:86
Deflection Temperature at 1.8 MPa (264 psi) 130 - 273 °C266 - 523 °FAverage value: 221 °C Grade Count:188
Deflection Temperature at 8.0 MPa 70.0 - 210 °C158 - 410 °FAverage value: 155 °C Grade Count:17
Minimum Service Temperature, Air -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:27
Glass Transition Temp, Tg 125 - 204 °C257 - 399 °FAverage value: 169 °C Grade Count:31
UL RTI, Electrical 105 - 170 °C221 - 338 °FAverage value: 131 °C Grade Count:67
UL RTI, Mechanical with Impact 130 - 170 °C266 - 338 °FAverage value: 133 °C Grade Count:67
UL RTI, Mechanical without Impact 130 - 170 °C266 - 338 °FAverage value: 133 °C Grade Count:31
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:203
Oxygen Index 22.0 - 66.0 %22.0 - 66.0 %Average value: 27.9 % Grade Count:28
Glow Wire Test 690 - 960 °C1270 - 1760 °FAverage value: 869 °C Grade Count:42
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 166 °C275 - 330 °FAverage value: 147 °C Grade Count:38
Nozzle Temperature 70.0 - 100 °C158 - 212 °FAverage value: 85.0 °C Grade Count:6
Melt Temperature 70.0 - 100 °C158 - 212 °FAverage value: 85.0 °C Grade Count:6
Mold Temperature 104 - 193 °C220 - 380 °FAverage value: 155 °C Grade Count:54
Injection Pressure 10.0 MPa1450 psiAverage value: 10.0 MPa Grade Count:6
Cure Time 0.167 - 0.667 min0.00278 - 0.0111 hourAverage value: 0.375 min Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass SMC
A. Schulman BMC 1901 Mineral Filled Alkyd
Overview of materials for Vinyl Ester Sheet Molding Compound
Plenco 08133 Polyester BMC, Compression Molded
Raschig Group RALUPOL® 2100 UP Polyester

O3509 / 78218

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.