MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ovako 20NiCrMoS2-2 4532 Steel, +QT
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel

Material Notes: General Information: Alloyed case hardening steel for very high strained parts and good toughness at core tensile strength of 700 - 900 MPa. Driving bevel gears, crown wheels, gears, shafts, bolts for automotive and gear components. Suitable for direct hardening.

Information provided by Ovako

Key Words: 20NiCrMo2-2, MoCN206 M, SAE 8620, BS 805H22, 20NCD2, SS2506
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 245
@Thickness 16.0 - 40.0 mm
>= 245
@Thickness 0.630 - 1.57 in
Round bar
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 400 °C752 °FMS
 723 °C1330 °FAC1
 827 °C1520 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.17 - 0.23 %0.17 - 0.23 %
Chromium, Cr 0.35 - 0.70 %0.35 - 0.70 %
Iron, Fe 96.82 - 98.28 %96.82 - 98.28 %As Balance
Manganese, Mn 0.60 - 0.95 %0.60 - 0.95 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Nickel, Ni 0.35 - 0.75 %0.35 - 0.75 %
Phosphorus, P 0.00 - 0.025 %0.00 - 0.025 %
Silicon, Si 0.10 - 0.25 %0.10 - 0.25 %
Sulfur, S 0.00 - 0.025 %0.00 - 0.025 %
 
Descriptive Properties
WeldabilityCEV 0.55max
 Pcm 0.32max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1095 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 50 mm (2 in.) round
Ovako 20NiCrMoS2-2 4548, MoCN 206 M Steel, +A
Ovako 20NiCrMoS2-2 4542 Steel, Hot forging
Ovako 20NiCrMoS2-2 4542 Steel, +QT
Ovako 20NiCrMoS2-2 4542 Steel, +A

NOVAKO160 / 234459

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.