Product Description: NAS XC is a styrene methyl methacrylate copolymer that can be used in a variety of applications demanding a extremely low haze and ultra clarity, also available with an UV package. Features: Sparking clarity; Low density; Easy of processing; Low moisture absorption Applications: Light Guide panels; Appliance partsAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Copolymer; Good Processability; High Clarity; Low Density; Low Moisture Absorption Uses: Appliance Components; Lighting Applications Appearance: Clear/Transparent Form: Pellets Processing Method: Injection Molding Information provided by INEOS Styrolution |