MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution NAS® XC SMMA
Categories: Polymer; Thermoplastic; Polystyrene (PS); Styrene/Methyl Methacrylate Copolymer (SMMA)

Material Notes: Product Description: NAS XC is a styrene methyl methacrylate copolymer that can be used in a variety of applications demanding a extremely low haze and ultra clarity, also available with an UV package.
Features: Sparking clarity; Low density; Easy of processing; Low moisture absorption
Applications: Light Guide panels; Appliance parts

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Copolymer; Good Processability; High Clarity; Low Density; Low Moisture Absorption

Uses: Appliance Components; Lighting Applications

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Injection Molding

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D792
Water Absorption at Saturation 0.17 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cmASTM D955
Melt Flow 1.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Tensile Strength, Yield 9300 psiASTM D638
Film Elongation at Break, MD 3.0 %ISO 527-3
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 470000 psiASTM D638
 493000 psiISO 527-1
Flexural Strength 14600 psiISO 178
 14900 psiASTM D790
Flexural Modulus 460000 psiASTM D790
 464000 psiISO 178
Izod Impact, Notched 0.400 ft-lb/inASTM D256
Charpy Impact Unnotched 9.70 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.670 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °FAnnealed; ISO 75-2/A
Vicat Softening Point 208 °FISO 306/B50
 221 °FRate B (120°C/h), Loading 1 (10 N); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54Sodium D Line; ASTM D542
Haze 0.30 %ASTM D1003
Transmission, Visible 93 %
@Thickness 14000 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 360 - 420 °F
Middle Barrel Temperature 390 - 450 °F
Front Barrel Temperature 410 - 470 °F
Melt Temperature 410 - 470 °F
Mold Temperature 90.0 - 140 °F
Drying Temperature 180 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYS770 / 311463

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.