MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röhm Plexiglas® 99560 MR2R Superclear Extruded, Mar Resistant PMMA Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: Description: PLEXIGLAS® Superclear 99560 MR2R is an extruded PMMA sheet with a mar resistant coating on both surfaces. The product has been developed for applications with highest demands on optical and surface quality. It has no observable haze, a very smooth surface, no light absorption and a very tight thickness tolerance.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiH961/30; ISO 2039-1
Tensile Strength at Break 72.0 MPa10400 psiISO 527-2/1B/5
 100 MPa
@Temperature -40.0 °C
14500 psi
@Temperature -40.0 °F
ISO 527-2/1B/5
Tensile Strength, Ultimate 35.0 MPa
@Temperature 70.0 °C
5080 psi
@Temperature 158 °F
ISO 527-2/1B/5
Elongation at Break 4.5 %4.5 %ISO 527-2/1B/5
Modulus of Elasticity 3.30 GPa479 ksiShort Term Value; ISO 527-2/1B/1
Flexural Strength 105 MPa15200 psi80x10x4 mm; ISO 178
Compressive Yield Strength 103 MPa14900 psiISO 604
Izod Impact, Notched (ISO) 1.60 kJ/m²0.761 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1fu
Abrasion <= 1.0<= 1.0% Haze, Abrasion resistance in Taber abrader test (100 rev.;5.4 N; CS-10F); ISO 9352
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDIN VDE 0303/3
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN VDE 0303/3
Dielectric Constant  2.8
@Frequency 100000 Hz
2.8
@Frequency 100000 Hz
DIN VDE 0303, Part 4
 3.7
@Frequency 50 Hz
3.7
@Frequency 50 Hz
DIN VDE 0303, Part 4
Dielectric Strength 30.0 kV/mm762 kV/inDIN VDE 0303, Part 2
Dissipation Factor  0.030
@Frequency 100000 Hz
0.030
@Frequency 100000 Hz
DIN VDE 0303, Part 4
 0.060
@Frequency 50 Hz
0.060
@Frequency 50 Hz
DIN VDE 0303, Part 4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
38.9 µin/in-°F
@Temperature 32.0 - 122 °F
DIN 53752A
Specific Heat Capacity 1.47 J/g-°C0.351 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 70.0 °C158 °F
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75
Vicat Softening Point 102 °C216 °FISO 306, Method B 50
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Flash Point 430 °C806 °FIgnition Temperature; DIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4911.491ISO 483
Haze <= 0.50 %<= 0.50 %ASTM D1003
Transmission, Visible >= 93 %>= 93 %DIN 5036, Part 3
UV Transmittance <= 1.0 %<= 1.0 %
Reflection Coefficient, Visible (0-1) 0.0330.033Reflection loss in the visible range (for each surface)
 
Descriptive Properties
Absorption in the Visible RangeMax 0.05%
Number of Inclusions (0.1 mm to 0.25 mm)Max 30 per m2Magnification Lens
Number of Inclusions (0.25 mm to 0.65 mm)Max 7 per m2Magnification Lens
Number of Inclusions (0.65 mm to 1.65 mm)Max 1 per m2Magnification Lens
Pencil Hardness6HASTM D3363, ISO 15184, KSD6711:1992 (Results may vary with different pencil sets.)
Sound Velocity2700-2800 m/sat room temperature
U Value for 1mm5.8 W/m2KDIN 4701
U Value for 2mm5.6 W/m2KDIN 4701

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® 99560 Superclear Extruded PMMA Sheet
Plaskolite Optix® Acrylic Sheet
Zeon Specialty Materials ZEONOR® 1410R Cyclo Olefin Polymer
Overview of materials for Polycarbonate, Extruded
Röhm Acrylite® AR Acrylic Sheet, Abrasion Resistant

PHUK042 / 47176

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.