MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EDRO #2 Prehardened 4130 Holder Block
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Chrome-moly Steel

Material Notes: EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition.
EDRO #2™ is characterized by excellent machinability, good resistance to indentation, and uniform hardness in all dimensions.
Applications: holders/bolsters for plastic molds and die-casting dies, plastics and rubber molds with low requirements on polishability, support plates, and constructional parts

Information provided by EDRO

Key Words: AISI 4130-35 improved
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 293 - 332293 - 332
Hardness, Vickers  650
@Treatment Temp. 525 °C
650
@Treatment Temp. 977 °F
Nitriding in ammonia gas
 700
@Treatment Temp. 570 °C
700
@Treatment Temp. 1060 °F
Tufftriding (Tenifer process)
Tensile Strength, Ultimate  793 MPa
@Temperature 399 °C
115000 psi
@Temperature 750 °F
Round bar 1" diameter, 310 HB
 951 MPa
@Temperature 199 °C
138000 psi
@Temperature 390 °F
Round bar 1" diameter, 310 HB
 1010 MPa
@Temperature 20.0 °C
146000 psi
@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
Tensile Strength, Yield  627 MPa
@Temperature 399 °C
91000 psi
@Temperature 750 °F
Round bar 1" diameter, 310 HB
 752 MPa
@Temperature 199 °C
109000 psi
@Temperature 390 °F
Round bar 1" diameter, 310 HB
 800 MPa
@Temperature 20.0 °C
116000 psi
@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
Elongation at Yield  18 %
@Temperature 20.0 °C
18 %
@Temperature 68.0 °F
in 2"
 20 %
@Temperature 199 °C
20 %
@Temperature 390 °F
in 2"
 23 %
@Temperature 399 °C
23 %
@Temperature 750 °F
in 2"
Reduction of Area  50 %
@Temperature 20.0 °C
50 %
@Temperature 68.0 °F
 52 %
@Temperature 199 °C
52 %
@Temperature 390 °F
 54 %
@Temperature 399 °C
54 %
@Temperature 750 °F
Charpy Impact  50.2 J
@Temperature 20.0 °C
37.0 ft-lb
@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
 55.6 J
@Temperature 199 °C
41.0 ft-lb
@Temperature 390 °F
Round bar 1" diameter, 310 HB
 71.9 J
@Temperature 399 °C
53.0 ft-lb
@Temperature 750 °F
Round bar 1" diameter, 310 HB
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.30 %0.30 %
Chromium, Cr 1.0 %1.0 %
Iron, Fe 96.72 %96.72 %As Balance
Manganese, Mn 1.1 %1.1 %
Molybdenum, Mo 0.20 %0.20 %
Silicon, Si 0.28 %0.28 %
Sulfur, S 0.40 %0.40 %
 
Descriptive Properties
Color CodeBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EDRO #7 Shock Resistant S7 Tool Steel
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
AISI 4130 Steel, normalized at 870°C (1600°F)
AISI 4130 Steel, water quenched 855°C (1570°F), 540°C (1000°F) temper, 100 mm (4 in.) round
EDRO P1FM #31 Free Machining Holder Steel

NSEDRO004 / 142941

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.