NOVA Chemicals Sclair® 14J1 Octene LMDPE Film Resin
(discontinued **)
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
Medium Density (MDPE)
;
Linear Medium Density Polyethylene (LMDPE), Film
Material Notes:
Film Properties. Features: Low gel, good clarity, high strength and toughness.
Applications:
Produce film.
Data provided by the manufacturer.
Key Words:
Linear Medium Density Polyethylene; Polyoctene; Polyolefin
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.934
g/cc
0.0337
lb/in³
ASTM D792
Melt Flow
0.72
g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.72
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
65
65
ASTM D2240
Film Tensile Strength at Yield, MD
15.0
MPa
2180
psi
ASTM D882
Film Tensile Strength at Yield, TD
17.0
MPa
2470
psi
ASTM D882
Film Elongation at Break, MD
650 %
650 %
ASTM D882
Film Elongation at Break, TD
820 %
820 %
ASTM D882
Secant Modulus, MD
0.400
GPa
58.0
ksi
ASTM D882
Secant Modulus, TD
0.500
GPa
72.5
ksi
ASTM D882
Coefficient of Friction
>= 0.50
>= 0.50
ASTM D1894
Elmendorf Tear Strength, MD
4.00
g/micron
102
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
14.0
g/micron
356
g/mil
ASTM D1922
Dart Drop
3.00
g/micron
76.2
g/mil
F 50; ASTM D1709/A
Film Tensile Strength at Break, MD
40.0
MPa
5800
psi
ASTM D882
Film Tensile Strength at Break, TD
39.0
MPa
5660
psi
ASTM D882
Thermal Properties
Metric
English
Comments
Vicat Softening Point
123
°C
253
°F
ASTM D1525
Brittleness Temperature
<=
-70.0
°C
<=
-94.0
°F
ASTM D696
Processing Properties
Metric
English
Comments
Melt Temperature
220
-
230
°C
428
-
446
°F
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Bayport Polymers Baystar™ Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film
ExxonMobil Exceed™ 2705 MC Film Grade Hexene LLDPE
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
PEHN0N / 35536
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.