MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Exceed™ 2705 MC Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Enable™ performance PE polymers allows film converters to further enhance their business with more stable operations, improve line output and down gauging — in one single polymer for mono- and coextrusion operations.  Enable™ 2705MC resins are ethylene 1-hexene copolymers.  This polymer offers an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior draw down and enhanced toughness.  TnPP is not intentionally added to Enable™2705 MC.   

Availability:   Africa & Middle East, Europe, North America, Asia Pacific, Latin America.  

Additive:  antiblock: no; slip: no; processing aid: yes; thermal stabilizer: yes. 

Applications:  food packaging, multilayer packaging film, shrink film, blown film, form fill and seal packaging, stand up pouches, heavy duty bags, collation shrink, lamination film, food packaging.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.1 MPa1900 psiASTM D882
Film Tensile Strength at Yield, TD 14.5 MPa2100 psiASTM D882
Film Elongation at Break, MD 520 %520 %ASTM D882
Film Elongation at Break, TD 760 %760 %ASTM D882
Puncture Energy 2.71 J2.00 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 50 g50 gASTM D1922
Elmendorf Tear Strength TD 730 g730 gASTM D1922
Dart Drop Test 130 g0.287 lbASTM D1709A
Film Tensile Strength at Break, MD 57.2 MPa8300 psiASTM D882
Film Tensile Strength at Break, TD 49.6 MPa7200 psiASTM D882
1% Secant Modulus, MD 303 MPa44000 psiASTM D882
1% Secant Modulus, TD 359 MPa52000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 °C246 °FPeak; ExxonMobil Method
Vicat Softening Point 114 °C237 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 11 %11 %ASTM D1003
Gloss 49 %49 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Bayport Polymers Baystar™ Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)

PEX98842 / 238226

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.