PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mechanical properties and is easy to injection mould. Applications: Injection moulded ESD products such as crates, boxes and tote bins for electronic components. Processing: PRE-ELEC® PP 1392 compound can be processed in the injection moulding machines using normal processing conditions as with polypropylene. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |