MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ascend Performance Materials HiDura™ PTR 840F Nylon PA66/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: HiDura PTR 840F is a polyamide copolymer that features good melt strength, flexibility, toughness, and slow crystallization. It offers melt viscosity and crystallization rate suitable for blown film, multi-bubble blown film, and thermoforming.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DAM; ISO 1183
Water Absorption 3.2 %
@Time 86400 sec
3.2 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption <= 0.100 %<= 0.100 %ASTM D 6869
Moisture Absorption at Equilibrium 2.7 %2.7 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 11 %11 %ISO 62
Viscosity Measurement 3.93.9Relative Viscosity; Sulfuric Acid; ISO 307
Linear Mold Shrinkage, Flow 0.014 cm/cm
@Thickness 2.00 mm
0.014 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm
@Thickness 2.00 mm
0.014 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 64.0 MPa9280 psi50% RH; ISO 527-2
 70.0 MPa10200 psiDAM; ISO 527-2
Elongation at Break 212 %212 %DAM; ISO 527-2
 386 %386 %50% RH; ISO 527-2
Tensile Modulus 0.627 GPa90.9 ksi50% RH; ISO 527-2
 2.30 GPa334 ksiDAM; ISO 527-2
Flexural Strength 14.0 MPa2030 psi50% RH; ISO 178
 74.0 MPa10700 psiDAM; ISO 178
Flexural Modulus 0.476 GPa69.0 ksi50% RH; ISO 178
 2.40 GPa348 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 4.20 kJ/m²
@Temperature -40.0 °C
2.00 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.30 kJ/m²
@Temperature 23.0 °C
2.05 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.80 kJ/m²
@Temperature -30.0 °C
2.28 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 5.80 kJ/m²
@Temperature -40.0 °C
2.76 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  16.4 J/cm²
@Temperature 23.0 °C
78.0 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 17.8 J/cm²
@Temperature -40.0 °C
84.7 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 17.9 J/cm²
@Temperature -30.0 °C
85.2 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.260 J/cm²
@Temperature -30.0 °C
1.24 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.270 J/cm²
@Temperature -40.0 °C
1.28 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.320 J/cm²
@Temperature -40.0 °C
1.52 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.330 J/cm²
@Temperature -30.0 °C
1.57 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.380 J/cm²
@Temperature 23.0 °C
1.81 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 4.20 J/cm²
@Temperature 23.0 °C
20.0 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  28.0 kV/mm
@Thickness 1.00 mm
711 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 28.0 kV/mm
@Thickness 1.00 mm
711 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 227 °C441 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C156 °FUnannealed; DAM; ISO 75-2/B
 120 °C248 °FUnannealed; 50% RH; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C117 °FUnannealed; DAM; ISO 75-2/A
 71.0 °C160 °FUnannealed; 50% RH; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 245 - 265 °C473 - 509 °FExtrusion
Zone 2 245 - 265 °C473 - 509 °FExtrusion
Zone 3 240 - 260 °C464 - 500 °FExtrusion
Zone 4 230 - 255 °C446 - 491 °FExtrusion
Zone 5 225 - 250 °C437 - 482 °FExtrusion
Die Temperature 245 - 265 °C473 - 509 °FExtrusion
Melt Temperature 245 - 265 °C473 - 509 °FExtrusion
 
Descriptive Properties
AdditiveLubricant
Agency RatingsASTM, D4066
 ASTM, D6779
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
AppearanceNatural Color
FeaturesChemical Resistant
 High Elongation
 High Impact Resistance
 High Melt Stability
 High Melt Strength
 High Strength
 High Toughness
 High Viscosity
 Lubricated
 Puncture Resistant
FormsPellets
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8606 / 293355

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.