MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
AISI 1026 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Machinability and weldability are fair. Cold formability of these steels is good to excellent. This grade responds favorably to heat treating and cold work.

Key Words: UNS G10260, ASTM A29, ASTM A273, ASTM A510, ASTM A519, ASTM A545, ASTM A576, carbon steels, SAE J403, SAE J412, SAE J414
Vendors:
Available Properties
  • Density, Chemical composition of 0.23% C, 0.635% Mn, 0.11% Si, annealed at 925°C
  • Hardness, Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity, Typical for steel
  • Bulk Modulus, Typical for steel
  • Poissons Ratio, Typical For Steel
  • Shear Modulus, Typical for steel
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Phosphorus, P
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.