Data provided by the manufacturer. 55 wt.% Bronze + 5 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable. |
Polytetrafluoroethylene; MoS2 |