  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Nouryon DEZ Diethylzinc
Categories: Other Engineering Material

Material Notes: DEZ is a chain transfer agent for molecular weight control in Ziegler-Natta polymerization of olefins. Also used as a scavenger to remove poisons from polyethylene reactors.

CAS number: 557-20-0

EINECS/ELINCS No.: 209-161-3

Applications: DEZ in low concentrations is an effective chain transfer agent for molecular weight control in Ziegler-Natta polymerization of olefins. It is useful in the production of polyethylene film with improved resistance to gelstreaking and pinstriping. It is also used as a scavenger to remove poisons from polyethylene reactors. DEZ has been used in a process for the preservation of books made with modern pulp-based paper. DEZ is also used in pharmaceutical applications where it is used mainly because stereo specifically reactions can be carried out. Well known is the Simmons-Smith cyclopropanation. DEZ is also useful in catalytic asymmetric addition to aldehydes or ketones forming chiral secondary or tertiary alcohols.

Information provided by Nouryon

Vendors:
Available Properties
  • Density
  • Viscosity
  • Molecular Weight
  • Heat of Vaporization, ?Hv, NBP
  • Specific Heat Capacity
  • Melting Point
  • Boiling Point
  • Heat of Formation, ?Hf°, 25 °C / 1 bar
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.