- Black: Kalix® 2955 BK 000
- White: Kalix® 2955 WH 000
Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; Platable
Uses: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts
Processing: Injection Molding; Water-Heated Mold Injection Molding
Availability: Asia Pacific; Europe; North America
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide