MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Chemours Tefzel™ ETFE HT-2188 Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Tefzel™ ETFE HT-2188 is a special purpose fluoroplastic resin available in translucent, 2.5-mm (0.1-in) pellets. Compared with other grades of Tefzel™ , it has a higher flow rate, low melting point, and high flexural endurance. Tefzel™ ETFE HT-2188 and the other Tefzel™ fluoroplastics are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. Tefzel™ ETFE HT-2188 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, such as tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts.

Information provided by Chemours.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Bulk Density, Chemours Test
  • Water Absorption, ASTM D270
  • Melt Flow, ASTM D3159
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D1457
  • Elongation, Ultimate, ASTM D638
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Flex Crack Resistance, ASTM D2176, Cycles MIT Folding Endurance
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D1531
  • Dielectric Strength, ASTM D150
  • Dissipation Factor, ASTM D1531
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air, UL 746
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.