Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CA 1110 G4 1740 is a 10% talc filled PP copolymer, with high melt flow, good impact resistance and excellent UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 1740 color version. Applications: Automotive Parts, Bumpers, Exterior Trim |