Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthalate blend for injection molding. It has improved surfac
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic