Temper: Hard Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Brazing, Butt Weld; Fair Suitability – Gas Shielded Arc Welding Common Fabrication Processes: Blanking, Coining, Coppersmithing, Drawing, Etching, Forming and Bending, Heading and Upsetting, Hot Forging and Pressing, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping Typical uses: Building Fronts; Downspouts; Flashing; Gutters; Roofing; Screening; Spouting; Gaskets; Radiators; Bus Bars; Commutator Segments; Contacts; Radio Parts; Switches; Terminals; Anodes; Chemical Process Equipment; Kettles; Pans; Printing Rolls; Road Bed Expansion Plates; Rotating Bands; Vats |