Available Properties |
---|
- Specific Gravity, ASTM D792, DAM
- Density, ISO 1183, DAM
- Filler Content, DAM
- Linear Mold Shrinkage, Flow, ISO 294-4, DAM
- Linear Mold Shrinkage, Transverse, ISO 294-4, DAM
- Tensile Strength at Break, ISO 527, 50%RH
- Tensile Strength at Break, ISO 527, DAM
- Tensile Strength, ASTM D638, 50%RH
- Tensile Strength, ASTM D638, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Tensile Stress at Strain, ISO 11403-1/-2, DAM
- Elongation at Break, ASTM D638, DAM
- Elongation at Break, ISO 527, DAM
- Elongation at Break, ASTM D638, 50%RH
- Elongation at Break, ISO 527, 50%RH
- Tensile Modulus, ISO 527, 50%RH
- Tensile Modulus, ISO 527, DAM
- Flexural Modulus, ASTM D790, 50%RH
- Flexural Modulus, ASTM D790, DAM
- Izod Impact, Notched, ASTM D256, DAM
- Izod Impact, Notched, ASTM D256, 50%RH
- Izod Impact, Notched (ISO), ISO 180/1A, DAM
- Izod Impact, Notched (ISO), ISO 180/1A, 50%RH
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, 50%RH
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Charpy Impact, Notched, ISO 179/1eA, 50%RH
- Comparative Tracking Index, UL 746A, DAM
- Comparative Tracking Index, UL 746A, DAM
- Melting Point, ISO 11357-1/-3, 10°C/min; DAM
- Melting Point, ASTM D3418, DAM
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, DAM
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
- UL RTI, Electrical, UL 746B, DAM
- UL RTI, Electrical, UL 746B, DAM
- UL RTI, Electrical, UL 746B, DAM
- UL RTI, Mechanical with Impact, UL 746B, DAM
- UL RTI, Mechanical with Impact, UL 746B, DAM
- UL RTI, Mechanical with Impact, UL 746B, DAM
- UL RTI, Mechanical without Impact, UL 746B, DAM
- UL RTI, Mechanical without Impact, UL 746B, DAM
- UL RTI, Mechanical without Impact, UL 746B, DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Flammability, UL94, UL94, DAM
- Flammability, UL94, UL94, DAM
- Flammability, UL94, UL94, DAM
- Melt Temperature, DAM; Optimum
- Melt Temperature, DAM
- Mold Temperature, DAM
- Mold Temperature, DAM; optimum
- Drying Temperature, DAM
- Dry Time, DAM
- Moisture Content, DAM
|
| | |